MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
CMW® 328 Copper Alloy  (discontinued **)
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: CMW® 328 material is a high strength, high conductivity copper base alloy. CMW® 328 is heat treatable. Optimum mechanical and physical properties of CMW® 328 material are developed by heat treatment or through a combination of heat treatment and cold working.

CMW® 328 material is used extensively for cap style resistance welding electrodes. Evidence suggests that it can provide less sticking and resist deformation longer than its copper-chrome counterpart (CMW® 3) in some specific situations. CMW® 328 can be substituted for CMW® 3 in any structural or current carrying situation without fear of degrading the design.

Information provided by CMW Inc.

1

Key Words: UNS C18150 (Wrought)
Vendors:
Available Properties
  • Density
  • Hardness, Rockwell B, Drawn Rod & Bar
  • Tensile Strength, Ultimate, Drawn Rod & Bar
  • Tensile Strength, Yield
  • Elongation at Break, Drawn Rod & Bar
  • Modulus of Elasticity, Bar, Rod & Strip
  • Electrical Resistivity, Bar & Rod (80% IACS)
  • CTE, linear
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Softening Point, Permanent Softening
  • Chromium, Cr
  • Copper, Cu
  • Zirconium, Zr
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
CMW Inc.

Category Notes
none

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.