MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Chemical Concepts PB-3 Siliconized Acrylic Latex
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: This premium quality one component, paintable, non-sag, low odor, mildew resistant siliconized acrylic latex sealant is formulated to provide a long lasting interior and exterior seal where slight to no movement is expected. Its creamy smooth consistency allows for ease in contractor tooling and cleanup of excess uncured sealant. The siliconized feature improves adhesion to many substrates including ceramic, glass, wood and plaster substrates. The final cured product provides for a watertight/weatherproof seal without the use of primers; ideal for applications such as windows, kitchens and bath fixtures. Features & Benefits: • Non-Sag • Low Odor • Paintable • Water Clean-Up • Exterior/Interior Use • Mildew Resistant • Non-Staining • Non Yellowing • Low Dirt.

Information provided by Chemical Concepts™.

Vendors:
Available Properties
  • pH
  • Viscosity Test, g/s
  • Vapor Pressure
  • Boiling Point
  • Flash Point, closed cup
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.