MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Master Bond EP30-D10 Abrasion Resistant, Flexible Adhesive Compound
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Master Bond Polymer System EP30-D10 is a versatile two component, abrasion resistant elastomer featuring superior strength, toughness and chemical resistance for high performance bonding, sealing, casting and encapsulation. It combines the performance characteristics of epoxy resins such as strength, chemical resistance, and adhesive qualities, with those of the polyurethanes including toughness, abrasion resistance and flexibility. In addition, EP30D10 has been used successfully in a number of different cryogenic applications. Master Bond Polymer System EP30D-10 is formulated to cure at room temperature or more rapidly at elevated temperatures. Master Bond Polymer System EP30D-10 is 100% reactive and does not contain any solvents or diluents. The Master Bond EP30D-10 system cures with minimal shrinkage to a durable, high strength, tough elastomer with good resistance to thermal cycling and chemicals including water, inorganic salts, alkalis and acids. It has an wide service temperature range of 4K to 220°F. Adhesion to metals, concrete, glass, ceramics, wood, vulcanized rubbers and many plastics is excellent. Color of part A is clear, part B is also clear. Master Bond Polymer System EP30D-10 is widely used in cryogenic, optical, electronic and aerospace applications both for original components and maintenance/repair. A non-drip version (amber colored) called EP30D-10ND is also available.

Product Advantages:

  • Long working life.
  • Versatile cure schedules; ambient temperature cures or fast cures at elevated temperatures as required.
  • High bonding strength to similar and dissimilar substrates including metals, rubbers, ceramics.
  • High impact strength, fatigue resistance and flexibility.
  • Low water absorption, low moisture permeability.
  • Superior retention of mechanical, chemical properties upon thermal cycling.
  • Excellent electrical insulation properties.
  • Temperature range,4K to 220°F; cryogenically serviceable.
  • 100% solids formulation; no solvents or diluents; minimal shrinkage upon curing.
  • Excellent optical properties; superior non-yellowing.

Information provided by MasterBond®

Vendors:
Available Properties
  • Viscosity, mixed
  • Hardness, Shore A
  • Tensile Strength at Break
  • Elongation at Break
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Pot Life, 100 gram batch
  • Shelf Life, in unopened container
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.