MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Matexcel ANT-0054 Antibacterial coating for glass
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: It is used for antibacterial coating on the surface of objects, which plays an important role in preventing bacterial infection and disease transmission. This product has the characteristics of high efficiency, broad spectrum and long-lasting. It can prevent the growth of a variety of bacteria. The appearance of the paint is colorless and transparent, and the antibacterial function is realized on the basis of retaining the original color and style of the substrate. This product is an antibacterial and antifungal coating specially designed for glass substrates. Water-based paint, safe and environmentally friendly, odorless; Colorless and transparent appearance, does not affect the color appearance of the substrate; Excellent adhesion; The antibacterial effect is strong, and the antibacterial rate of large intestine, golden grape, Bai Nian, etc. is over 99%; Good anti-mold performance, no detection of Aspergillus flavus, Aspergillus niger, Aspergillus syringae, Chaetomium globosum, etc. Long-lasting efficacy, ultraviolet light irradiation for more than 100 hours, antibacterial does not decay; The method of use is flexible and can be cured at room temperature.

Application: Used on the surface of glass substrates, such as hospitals, hotels, schools, kindergartens, office buildings, stations, docks, public transportation and other places, to purify the air, clean the environment, reduce the chance of cross infection, and improve the prevention of infectious diseases The role of protecting medical staff, people with weak constitution, preventing the invasion of bacteria and preventing the growth of mold.

Morphology: Colorless transparent liquid

Uses: Depending on the shape, size and surface condition of the substrate, suitable methods such as shower coating, dip coating, wiping, spraying, etc. should be selected for construction. It is recommended to test in a small area before construction. Step 1: Coating. Choose a suitable process for coating. Step 2: Curing at room temperature. In a normal temperature environment, the surface is dried for 20 minutes, and the coating is completely dried after 3 days. 1. Sealed and stored in a cool place with clear labels to prevent misuse and misuse; 2. Keep away from fire and heat sources, and keep it out of the reach of children; 3. The workplace should have good ventilation conditions, and fireworks are strictly prohibited; 4. It is recommended that operators wear work protective clothing, chemical protective gloves, and goggles; 5. Prohibit entrance, avoid contact with eyes and skin. In case of splashing into eyes, immediately rinse with plenty of water and seek medical advice.

Key Words: Antibacterial coating for glass
Vendors:
Available Properties
  • Storage Temperature, Storage in a cool, dry place, avoid direct sunlight.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.