REPOL Polypropylene H029SG is being manufactured using Unipol PP process, which combines the production efficiency of gas phase fluidized bed reactor with the high activity stereospecific catalyst system. Repol H029SG is recommended for use in Oriented Film process. Repol H029SG is the material of choice for BOPP films used in adhesive tapes, food packaging, cigarette & textile overwraps, lamination, synthetic paper etc. Features: High tensile strengthExcellent gloss and clarityGood processabilityInformation provided by Reliance Industries |