MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Röchling GLASROD® Grade SG-200 Solid Rod and Bar
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Grade SG-200: Highest temperature – UL-rated for 210°C service. Grade SG-200 is a recognized component in UL listed Insulation systems for temperature rating of up to 200°C. Excellent thermal endurance. Ideal replacement for silicone rod. Available in Rectangular, Square “A” and Dogbones shapes. All GLASROD® solid rod and bar products features:
  • High physical strength
  • Excellent dielectric properties
  • Dimensional stability
  • Resistance to common solvents
  • Heat resistance
  • High strength-to-weight ration
  • Low water absorption
GLASROD® solid rod and bar products are fiberglass-reinforced thermoset polyester shapes which exhibit properties desirable for a wide range of structural and electrical applications. Superior strength provided by the continuous filament fiberglass roving is complemented by the physical and electrical characteristics contributed by the thermoset polyester resins. Together they provide the right combination of properties to offer significant price/performance advantages over alternative materials.

Information provided by Röchling.

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ASTM D570
  • Tensile Strength, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Strength, ASTM D695, transverse
  • Compressive Strength, ASTM D695, axial
  • Izod Impact, Notched, ASTM D256
  • Insulation Resistance
  • Dielectric Constant
  • Arc Resistance, ASTM D495
  • CTE, linear, ASTM D696
  • Thermal Conductivity, ASTM C177
  • Flammability, UL94
  • Oxygen Index, ASTM D2863
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.