Notes: A highly engineered thermoplastic material for use as an ultra-thin coextruded layer in demanding applications requiring, superior low friction and abrasion resistance properties. Lubmer TM-80B is a UV stable grade possessing exceptional friction and abrasion performance. TM-80B is engineered to have outstanding adhesion to Sarlink TPV materials create effective system for vehicle sealing applications such as glass run channels, waist belts, auxiliary seals, and other profiles or articles. Availability: Europe; Asia Pacific; Latin America; North America Features: High Stiffness; High Strength; Low Density Uses: Bearings; Machine/Mechanical Parts Processing Method: Injection Molding Features: Chemical Resistant; Good Adhesion; High Hardness; High Heat Resistance; High Slip; Low Compression Set; Low Density; Low Friction; Low Specific Gravity; UV Resistant Uses: Automotive Applications; Automotive Exterior Parts; Automotive Window Encapsulation; Rubber Replacement RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Extrusion Information provided by Teknor Apex |