MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Renegade Materials Corporation RM-5001 Cyanate Ester Prepreg, 6781 S2 Glass Fabric
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset

Material Notes: RM-5001 cyanate ester is a very low outgassing, toughened, high performance prepreg.

  • Straightforward 350°F Cure
  • Designed for the unique requirements of satellite and missile structures
  • Low shrinkage during cure
  • Developed for consistent handling and superior performance
  • Continuous service up to and including 350°F with post cure
  • Available in woven and unidirectional product forms using all fibers including carbon, quartz and S2 glass
  • Nano-enhancement for tailored laminate properties and multi-functional performance
  • Low moisture absorption

    Information provided by Renegade Materials Corporation.

    Renegade Materials has been acquired by Teijin.

  • Vendors:
    Available Properties
    • Density, Resin
    • Moisture Absorption at Equilibrium, Post cured at 350°F
    • Moisture Absorption at Equilibrium, Post cured at 450°F
    • Tensile Strength, Ultimate, ASTM D3039, Prepreg, Warp Direction, RT, Dry, Normalized to 60% fiber volume fraction
    • Elongation at Break, Resin
    • Tensile Modulus, ASTM D3039, Prepreg, Warp Direction, RT, Dry, Normalized to 60% fiber volume fraction
    • Flexural Strength, Resin, RT, Wet
    • Flexural Strength, Resin, RT, Dry
    • Flexural Strength, ASTM D7264, Prepreg, Warp Direction, RT, Dry, Normalized to 60% fiber volume fraction
    • Flexural Modulus, ASTM D6272, Resin, RT, Dry
    • Flexural Modulus, Resin, RT, Wet
    • Flexural Modulus, ASTM D7264, Prepreg, Warp Direction, RT, Dry, Normalized to 60% fiber volume fraction
    • Shear Strength, ASTM D2344, Interlaminar, RT, Dry
    • Dielectric Constant
    • Dissipation Factor
    • Maximum Service Temperature, Air
    • Glass Transition Temp, Tg, Resin, Wet, Cured at 450°F
    • Glass Transition Temp, Tg, Resin, Dry, Cured at 350°F
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    none

    Category Notes
    Plastic

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Rulon Bearings
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.