MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
SABIC NORYL™ Resin PX9406P Polyphenylene Ether + PS (PPE+PS) (Asia)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ PX9406P resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of 5VA at 2.5mm and V0 at 0.75mm. NORYL PX9406P is VDE certified IEC60335 and offers strong electrical performance at thin wall, high heat resistance, Low Warpage, low moisture absorption, and dimensional stability. This material is an excellent candidate for unattended appliance applications such as printed circuit board (PCB) holders, terminal blocks + connectors, circuit protection / relay / switches, motor end caps, control box / panels, and battery charger / fuse holders where VDE IEC60335 is required.

Features: Hydrolytic Stability,Low Creep Sensitivity,Non-Halogenated,Non-Chlorinated,Non-Brominated,Low Warpage

Information provided by SABIC

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Density, ISO 1183
  • Water Absorption, ASTM D570
  • Moisture Absorption, Injection Molding
  • Viscosity, ISO 11443, melt
  • Viscosity, ISO 1133, MVR cc/10 min
  • Linear Mold Shrinkage, Flow, SABIC method
  • Melt Flow, ASTM D1238
  • Tensile Strength, Yield, SABIC - Japan Method
  • Tensile Strength, Yield, ISO 527, 50 mm/min
  • Elongation at Break, ISO 527, 50 mm/min
  • Elongation at Break, SABIC - Japan Method
  • Flexural Strength, ASTM D790
  • Flexural Strength, ISO 178, yield, 2 mm/min
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ISO 178, 2 mm/min
  • Izod Impact Notched, ASTM D256
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4
  • Charpy Impact Unnotched, ISO 179/1eU, Edgew 80*10*4 sp=62mm
  • Charpy Impact, Notched, ISO 179/1eA, Edgew 80*10*4 sp=62mm
  • Surface Resistance, ASTM D257
  • Dielectric Constant, ASTM D150
  • Arc Resistance, ASTM D495
  • Comparative Tracking Index, UL 746A
  • Hot Wire Ignition, HWI, UL 746A
  • High Amp Arc Ignition, HAI, UL 746A
  • High Voltage Arc-Tracking Rate, HVTR, UL 746A
  • CTE, linear, TMA
  • CTE, linear, Parallel to Flow, ISO 11359-2
  • CTE, linear, Transverse to Flow, ISO 11359-2
  • Hot Ball Pressure Test, IEC 60695-10-2
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75/Af, Flatw 80*10*4 sp=64mm
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, unannealed
  • Vicat Softening Point, ISO 306, Rate B/120
  • Vicat Softening Point, ISO 306, Rate A/120
  • UL RTI, Electrical, UL 746B
  • UL RTI, Mechanical with Impact, UL 746B
  • UL RTI, Mechanical without Impact, UL 746B
  • Flammability, UL94, UL 94
  • Flammability, UL94, UL 94
  • Flammability, UL94, UL 94
  • Flammability, UL94, UL 94
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Flammability Index, IEC 60695-2-12
  • Glow Wire Flammability Index, IEC 60695-2-12
  • Glow Wire Flammability Index, IEC 60695-2-12
  • Glow Wire Flammability Index, IEC 60695-2-12
  • Nozzle Temperature
  • Zone 2
  • Zone 3
  • Melt Temperature, Injection Molding
  • Mold Temperature
  • Drying Temperature, Injection Molding
  • Dry Time, Injection Molding
  • Dry Time, Cumulative; Injection Molding
  • Back Pressure
  • Shot Size
  • Vent Depth
  • Screw Speed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saudi Basic Industries Corporation; SABIC Innovative Plastics (GE Plastics)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.