MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Angst+Pfister APSOplast® PPS SL PPS + carbon fibre + graphite + PTFE
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler

Material Notes: This semi-crystalline polymer is filled with carbon fibre, graphite, and PTFE. It is very rigid and hard as well as having exceptional sliding and friction properties. The service temperature of up to +220 °C, very good chemical resistance, low creep tendency, and high dimensional stability enable applications for components which are exposed to high thermal and static/dynamic loads in the fields of pumps, fittings, vacuum technology, packaging machines, paper machines, precision engineering, aeronautics, and astronautics.

Information provided by Angst + Pfister

Vendors:
Available Properties
  • Density, DIN EN ISO 1183-1
  • Water Absorption, DIN EN ISO 62
  • Water Absorption, DIN EN ISO 62
  • Moisture Absorption, DIN EN ISO 62, at saturation in standardized climate
  • Ball Indentation Hardness, DIN EN ISO 2039-1
  • Tensile Strength at Break, DIN EN ISO 527, 50 mm/min
  • Tensile Strength, DIN EN ISO 527
  • Tensile Strength, Yield, DIN EN ISO 527
  • Elongation at Break, DIN EN ISO 527
  • Elongation at Yield, DIN EN ISO 527, 50 mm/min
  • Modulus of Elasticity, DIN EN ISO 527, tensile test
  • Modulus of Elasticity, DIN EN ISO 178, flexural test
  • Flexural Strength, DIN EN ISO 178
  • Compressive Strength, EN ISO 604, 5 mm/min
  • Compressive Strength, EN ISO 604, 5 mm/min
  • Compressive Modulus, EN ISO 604
  • Charpy Impact Unnotched, DIN EN ISO 179-1eU
  • Volume Resistivity, DIN EN 61340-2-3
  • Surface Resistance, DIN EN 61340-2-3
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point, ISO 11357-3
  • Maximum Service Temperature, Air, long term
  • Maximum Service Temperature, Air, short term
  • Deflection Temperature at 1.8 MPa (264 psi), DIN EN ISO 75 / A
  • Glass Transition Temp, Tg, DIN 53765
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.