MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Schmolz + Bickenbach 430FR Stainless Steel Bar
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Description: Ugitech’s 430FR is a ferritic stainless steel designed for soft magnetic components operating in corrosive environments. The 17.00% - 18.00% chromium makes corrosion resistance similar to 430F. The increased silicon content in this alloy allows increased magnetic characteristics over 430F in the annealed condition. 430FR has exhibited superior and consistent performance due to its higher electrical resistivity. The alloy was developed for applications that require a weak coercive magnetic force (Hc =1.88 – 3.00 Oe [150 – 240 A/m]) as needed in solenoid valves. Our controlled processing allows magnetic properties to be typically superior to industry norms. 430FR has an increased hardness over 430F, due to the increased silicon levels, reducing the deformation that occurs during the oscillation impacts that occur in AC and DC solenoid valves

Applications: Solenoid Valves and Injectors

Information provided by Schmolz + Bickenbach

Key Words: ASTM A838 Alloy 2; EN 10088-3 1.4105, X6CrMoS17
Vendors:
Available Properties
  • Density
  • Hardness, Brinell, Magnetically Annealed (Grade 1)
  • Tensile Strength, Magnetically Annealed (Grade 1)
  • Tensile Strength, Yield, Magnetically Annealed (Grade 1)
  • Elongation at Yield, Magnetically Annealed (Grade 1)
  • Reduction of Area, Magnetically Annealed (Grade 1)
  • Tensile Modulus
  • Magnetic Permeability, [µ]
  • Magnetic Permeability, [µ]; Typical delivered
  • Magnetic Coercive Force, Hc, [µ]
  • Magnetic Coercive Force, Hc, [µ]; Typical delivered
  • Magnetic Saturation Flux Density, Bmax
  • Magnetic Remanence, Br
  • Magnetic Remanence, Br, Typical delivered magnetic properties
  • CTE, linear
  • Thermal Conductivity
  • Annealing Temperature, For softening
  • Annealing Temperature, Optimum magnetic properties; Then cool to 930°F at a rate of 120°F per hour
  • Annealing Temperature, Then cool to 930°F at a rate of 120°F per hour
  • Hot-Working Temperature, Uniformly heating
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Schmolz + Bickenbach (Swiss Steel International)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.