MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Ineos R55C-00 Clarified Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Grade R55C-00 is a high melt flow rate clarified and antistatic random polypropylene copolymer. It is designed for high speed injection molding of thin walled parts requiring very good mold filling capabilities, excellent clarity, fast cycle times and good stiffness-to-impact properties balance. This material meets the requirements of the US Food and Drug Administration as specified in 21 CFR 177.1520. Preliminary properties listed below could later be subject to minor change.
    Applications:
  • Thin wall injection molding (TWIM) of multi-cavity parts
  • Stadium cups and containers
  • Audio/video media rigid packaging formats
  • Consumer products and housewares
    Benefits:
  • High flow rate for easier mold filling
  • High clarity in thin-walled parts
  • Fast cycling
  • Low bloom and good static charge dissipation
  • Very good impact resistance

    Information provided by Ineos Olefins & Polymers USA

Key Words: Excellent clarity, fast cycle times and good stiffness-to-impact properties balance
Vendors:
Available Properties
  • Melt Flow, ASTM D1238
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength, Yield, ASTM D638
  • Flexural Modulus, ASTM D790A
  • Izod Impact, Notched, ASTM D256, 1/8" (3mm) notched bar
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Transmission, Visible, ASTM D1003, plaque, Diffuse Transmittance
  • FDA, See notes for details.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Ineos Olefins & Polymers USA

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.