MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
NOVA Chemicals Surpass® RMs244-UG Octene sHDPE Rotational Molding Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Rotational Molding Grade

Material Notes:

Features:

  • Octene copolymer
  • Exceptional low temperature properties
  • Outstanding stiffness
  • Broad processing window
  • Superior whiteness for improved part appearance
  • Easy mold release
  • NSF listed for Standards 14, 24 and 61
  • Applications:

  • Custom Industrial parts
  • Storage tanks
  • Marine products
  • Materials handling containers
  • Information provided by Nova Chemicals

    Vendors:
    Available Properties
    • Density, ASTM D792, Compression Molded
    • ESCR 10% Igepal®, ARM Method, Compression Molded
    • Melt Flow, ASTM D1238, Compression Molded
    • Tensile Strength, Yield, ASTM D638, Compression Molded
    • Tensile Strength, Yield, ASTM D882, Rotational Molded
    • Flexural Modulus, ASTM D790, Rotational Molded
    • Flexural Modulus, ASTM D790, Compression Molded
    • Impact Test, ARM Method, Compression Molded
    • Melting Point, ASTM E794, Compression Molded
    • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Compression Molded
    • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Compression Molded
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    none

    Category Notes
    Plastic

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Rulon Bearings
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.