Processing: Molding, Extrusion and Forming Applications: Thermoformed food and non-food packaging, extruded profile, plates, dishes, disposable cups, and deep drawn thermoformed containers. Also suitable for audio/ visual cabinets, business machines, and toys. MARPOL® PSH 6054 can - in principle - be used in food contact applications in the USA (FDA) and in Canada (HBP). Migration or use limitations may apply. Information provided by Marco Polo International, LLC |