MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
American Utility Metals Cromgard® Stainless Steel
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits of strength, corrosion and abrasion resistance, durability and low maintenance.

Cromgard generally conforms to ASTM A240 UNS S41003. Additionally, it can be certified to European standard EN 10088-2 type 1.4003. It is also included in the specification EN 10028-7 for stainless steels suitable for pressure purposes, which includes minimum specified impact values.

The substantially austenitic microstructure at elevated temperatures also restricts grain growth during welding. This leads to a tough duplex martensitic/ferritic heat affected zone, responsible for good weldability.

Key Words: UNS S41003
Vendors:
Available Properties
  • Density
  • Hardness, Brinell, per ASTM A240
  • Tensile Strength, per ASTM A240; transverse
  • Tensile Strength, Ultimate, Typical annealed sample; short time elevated temp.
  • Tensile Strength, Ultimate, Typical annealed sample; short time elevated temp.
  • Tensile Strength, Ultimate, Typical annealed sample; short time elevated temp.
  • Tensile Strength, Ultimate, Typical annealed sample; short time elevated temp.
  • Tensile Strength, Ultimate, Typical annealed sample; short time elevated temp.
  • Tensile Strength, Yield, Typical annealed sample; short time elevated temp.
  • Tensile Strength, Yield, Typical annealed sample; short time elevated temp.
  • Tensile Strength, Yield, Typical annealed sample; short time elevated temp.
  • Tensile Strength, Yield, Typical annealed sample; short time elevated temp.
  • Tensile Strength, Yield, Typical annealed sample; short time elevated temp.
  • Tensile Strength, Yield, per ASTM A240; transverse; 0.2% Proof
  • Tensile Strength, Yield, per ASTM A240; transverse
  • Elongation at Break, per ASTM A240; transverse
  • Creep Strength, time to produce 1% strain
  • Creep Strength, time to produce 1% strain
  • Creep Strength, time to produce 1% strain
  • Creep Strength, time to produce 1% strain
  • Creep Strength, time to produce 1% strain
  • Creep Strength, time to produce 1% strain
  • Creep Strength, time to produce 1% strain
  • Creep Strength, time to produce 1% strain
  • Creep Strength, time to produce 1% strain
  • Creep Strength, time to produce 1% strain
  • Creep Strength, time to produce 1% strain
  • Creep Strength, time to produce 1% strain
  • Modulus of Elasticity, Typical annealed sample; short time elevated temp.
  • Modulus of Elasticity, Typical annealed sample; short time elevated temp.
  • Modulus of Elasticity, Typical annealed sample; short time elevated temp.
  • Modulus of Elasticity, Typical annealed sample; short time elevated temp.
  • Modulus of Elasticity, Typical annealed sample; short time elevated temp.
  • Tensile Modulus
  • Poissons Ratio
  • Fatigue Strength
  • Fatigue Strength
  • Fatigue Strength
  • Fatigue Strength
  • Shear Modulus
  • Charpy Impact, to EN 10028-7 1.4003
  • Electrical Resistivity
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Maximum Service Temperature, Air, Continuous
  • Maximum Service Temperature, Air, Intermittent
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, Remainder
  • Manganese, Mn
  • Nickel, Ni
  • Nitrogen, N
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.