Filler/Reinforcement: Glass Fiber, 30% Filler by Weight
Additive: Impact Modifier
Features: Impact Modified
RoSH Compliance: RoSH Compliant
Automotive Specifications: ASTM D4066 PA026 G30 Color: 9922 Black; GM GMW15702-023141 PA6-HI-GF30 Color: 9922 Black; PSA Peugeot-Citroen SPA X62 4119 Color: 9922 Black
Forms: Granules
Processing Method: Injection Molding