MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
CMW® 3 Copper Alloy  (discontinued **)
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: CMW® 3 material is a high strength, high conductivity copper base alloy. CMW® 3 material is heat treatable. Optimum mechanical and physical properties of CMW® 3 material are developed by heat treatment or through a combination of heat treatment and cold working.

CMW® 3 material is used extensively for spot welding electrodes and is well suited for custom bent designs, flash welding dies, and seam welding wheels, and provides better performance and greater savings than other copper alloys used for spot and seam welding.

Property data for fully precipitation heat treated condition.

Information provided by CMW Inc.

1

Key Words: UNS C18200 (Wrought); UNS C18500 (Cast)
Vendors:
Available Properties
  • Density
  • Hardness, Rockwell B, Forging (Hot Forged and Heat Treated)
  • Hardness, Rockwell B, Premium Casting
  • Hardness, Rockwell B, Premium Forging (Hot Forged, Heat Treated, and Cold Worked to less than 1" thick)
  • Hardness, Rockwell B, Strip (TH04)
  • Hardness, Rockwell B, Plate
  • Hardness, Rockwell B, Drawn Rod & Bar
  • Tensile Strength, Ultimate, Premium Casting
  • Tensile Strength, Ultimate, Forging (Hot Forged and Heat Treated)
  • Tensile Strength, Ultimate, Premium Forging (Hot Forged, Heat Treated, and Cold Worked to less than 1" thick)
  • Tensile Strength, Ultimate, Strip (TH04)
  • Tensile Strength, Ultimate, Plate
  • Tensile Strength, Ultimate, Drawn Rod & Bar
  • Tensile Strength, Yield, Premium Casting
  • Tensile Strength, Yield, Forging (Hot Forged and Heat Treated)
  • Tensile Strength, Yield, Premium Forging (Hot Forged, Heat Treated, and Cold Worked to less than 1" thick)
  • Tensile Strength, Yield, Strip (TH04)
  • Tensile Strength, Yield, Plate
  • Tensile Strength, Yield, Drawn Rod & Bar
  • Elongation at Break, Strip (TH04)
  • Elongation at Break, Premium Forging (Hot Forged, Heat Treated, and Cold Worked to less than 1" thick)
  • Elongation at Break, Premium Casting
  • Elongation at Break, Forging (Hot Forged and Heat Treated)
  • Elongation at Break, Plate
  • Elongation at Break, Drawn Rod & Bar
  • Reduction of Area, Premium Casting
  • Reduction of Area, Premium Forging (Hot Forged, Heat Treated, and Cold Worked to less than 1" thick)
  • Reduction of Area, Forging (Hot Forged and Heat Treated)
  • Reduction of Area, Drawn Rod & Bar
  • Modulus of Elasticity, Bar, Rod & Forgings
  • Modulus of Elasticity, Castings & Strip
  • Modulus of Elasticity, Plate
  • Electrical Resistivity, Bar, Rod & Forgings (85 % IACS)
  • Electrical Resistivity, Castings & Strip (80 % IACS)
  • Electrical Resistivity, Plate (78 % IACS)
  • CTE, linear
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Softening Point, Permanent Softening
  • Chromium, Cr
  • Copper, Cu
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
CMW Inc.

Category Notes
none

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.