MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Syensqo (Solvay Specialty Polymers) Cogegum® GFR/370 Polyolefin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefin base containing a fire retardant system that contributes to give the cable self-extinguish properties without halogenidric acids evolution, toxic and corrosive gases and dark smoke emission. This material complies with RoHS requirements. Standard complying - EN 50363-6 EM8, EM10; EN 50264 EM101..104; IEC 60092 SHF2; VDE 0207 HM3

Additional Information: Tests reported are performed on pressed or extruded specimens, added with 3% of Catalyst CT/2-MD UV and crosslinked in hot water at 95°C for 6 hours Coloring - EVA or PE based masterbatches added at 1.2-1.5% by weight; in order to avoid scotching problems during processing, predrying of colour masterbatch is suggested if moisture absorption occurred during storage (4-6 hours at 50-60°C). Storage - The product must be stored under the following conditions: -- closed and unteared bags -- ambient temperature not exceeding 35°C -- avoid direct exposure to sunlight and weathering - Product alterations could occur due to extended period of storage - Shelf life: 6 months - Solvay Specialty Polymers accepts no liability of any kind in case the above mentioned conditions are not fulfilled. Packaging - 25 kg moisture-resistant bags on 1375 kg pallet - 1000 kg carton box

Extrusion Notes: Processing - COGEGUM® GFR/370 pregrafted base must be added with Catalyst CT/2-MD UV masterbatch to promote curing. Catalyst dosage is 3% by weight and blending must be done just before using (2-3 hours max.), preferably in the extruder hopper. Catalyst doesn't need any predrying if stored in dry conditions in the original closed bags; in case, predrying can be made at 50-60°C for 4-8 hours - The pregrafted base compound is sensible to moisture; open bags must be used within 4 hours. Pregrafted base cannot be predried Extrusion equipment - standard extruders for thermoplastics equipped with low compression screw (1:1.2-1.4 compression ratio and 25 L/D ratio are suggested), and an adequate barrel thermoregulation - don't use screw thermoregulation - filter net: none - compression tools suggested Curing - by immersion in hot water at 60-70°C - by exposure in ambient, crosslinking time depends on ambient temperature and relative humidity - in all cases curing time depends on insulation thickness; for 0.7-1.2 mm wall thickness 3-6 hours are generally necessary in case of forced curing in hot water

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • ESCR 10% Igepal®, ASTM D1693, Condition A, Compression Molded
  • Melt Flow, Internal Method, without Catalyst MB addition
  • Hardness, Shore D, ISO 868
  • Tensile Strength at Break, IEC 60811
  • Elongation at Break, IEC 60811
  • Maximum Service Temperature, Air, NES 715, Temperature Index (Burning)
  • Oxygen Index, ASTM D2863
  • Processing Temperature, Collar Temperature
  • Zone 1
  • Zone 2
  • Zone 3
  • Zone 4
  • Die Temperature
  • Head Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.