MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Hybrid Plastics MS0825 Nanoreinforced® POSS® Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Nanoreinforced® polypropylene utilizes POSS® technology to achieve, increased hydrophobicity, lower coefficient of friction and improved processability through structural control at the nanometer level. These enhancements can be realized in any grade of PP and are controlled by the nanoscopic size and reliable dispersion of POSS cages throughout the resin.

Enhanced hydrophobicity: The hydrophobic properties of POSS® synergistically combines with PP morphology to create a nano-rough surface that is both hydrophobic and low friction. The technique is ideally suited to masterbatching. Enhanced hydrophobicity is observed by water contact angle differences for PP and Nanoreinforced® PP. Water contact angle increases with POSS® content, and follows standard rules of mixing when let down from a masterbatch.

A Low Friction Surface results at the nanometer scale. A four times increase in surface roughness is caused by the POSS® cages. This effectively reduces the contacted surface area, leading to a significant decrease in coefficient of friction. Coefficient of friction (µ) decreases of 60% can be realized by incorporation of POSS and can be controlled by the let down of a masterbatch. For example: PP µ = 0.17, 5% POSS® PP = µ 0.14, 10% POSS® PP µ = 0.07, Teflon® µ = 0.03.

Faster processing results from a lubricity effect thatis imparted by the POSS and increases melt flow and decreases the screw torque required during compounding and during masterbatch let down. Suggested Applications as a low-cost replacement for fluorinated and silicone resins.

Vendors:
Available Properties
  • Melt Flow, 5% POSS® in PP
  • Melt Flow, 10% POSS® in PP
  • Coefficient of Friction, 10% POSS® in PP
  • Coefficient of Friction, 5% POSS® in PP
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.