Shielding - Glass Fiber 15% - Stainless Steel Fiber 5% - Flame Retardant Comments: - EMI/RFI Shielding
- ESD Protection
- Glass Fiber
- Stainless Steel Fiber
- Flame Retardant
Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties. Information provided by RTP Company. Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade. |