EY2562 is designed to fill the need for a strong, pourable and lightweight filler for honeycomb core panels. It can be used to pot fasteners or as edge closeout after the panel is trimmed to contour. It is fire retardant, resistant to long exposure to 350°F and cures at room temperature in thicknesses in excess of one inch. Features and Benefits: - Extremely Light Weight
- Excellent Chemical Resistance
- Self Extinguishing
- Excellent Bonding to Metals, Composites, Coatings, and Most Plastics
- Excellent Chemical Resistance
- Suitable for MMD Dispensing Equipment
- Excellent Thermal Performance
- Room Temperature Cure
Information provided by H.B. Fuller Company |