Temper: Hard Fabrication Properties: Excellent Suitability – Soldering, Brazing, Oxyacetylene Welding, Gas Shielded Arc Welding, Butt Weld, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Good Suitability – Coated Metal Arc Welding; Fair Suitability – Spot Weld Typical uses: Welding Rod and Wire; Artillery Projectile Rotating Bands, Welded Applicable Specifications: Electrode – Welding MILITARY MIL-E-45829, Welding AWS A5.6; Rod – Welding AWS A5.7 |