MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
CeramTec CeramCool® Rubalit® 708 Alumina, 96%
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivity, thermal cycling stability, high breakthrough voltage, no corrosion, and no water intrusion. Benefits of CeramCool®: optimized thermal management, passive cooling, absorption of thermal stress, increased lifetime of die, higher color stability, reduction TCE mismatch, thermal expansion coefficient of semiconductor materials, one system for alignment of sources, simplified system, miniaturization, weight reduction, cost reduction, and high current conductors. CeramCool® can be metallized directly with thick or thin film processes such as conventional ceramic substrates. This makes the complete surface of the heat-sink useable as a circuit carrier while providing reliable electrical insulation. CeramCool® is available from the proven ceramic material Rubalit® 708. This material has a thermal expansion coefficient that is adapted to semi-conductor materials, possesses excellent electrical characteristics and is at the same time corrosion-resistant. CeramCool® is available with or without metallizations.

Key Words: Al2O3, aluminum oxide
Vendors:
Available Properties
  • Density, ASTM-C20
  • Water Absorption, ASTM-C373
  • Particle Size, Medium Grain (d50)
  • Modulus of Elasticity, ASTM-F417
  • Flexural Strength, ASTM-F417, Bending Strength; 4-point method (40x4x3 mm³)
  • Flexural Strength, DIN 52292, Bending Strength; dual-ring method (0.63 mm substrate thickness)
  • Volume Resistivity, ASTM-D257
  • Volume Resistivity, ASTM-D257
  • Volume Resistivity, ASTM-D257
  • Volume Resistivity, ASTM-D257
  • Dielectric Constant
  • Dielectric Constant
  • Dielectric Breakdown, ASTM-D149
  • Dielectric Breakdown, ASTM-D149
  • Dielectric Breakdown, ASTM-D149
  • Dielectric Loss Index, ASTM-D150
  • CTE, linear, ASTM-C372
  • CTE, linear, ASTM-C372
  • CTE, linear, ASTM-C372
  • Specific Heat Capacity
  • Thermal Conductivity, ASTM-C408
  • Al2O3
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
CeramTec North America

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.