Heat treatment: 975 °C, 1/2 hour, AC and 595 °C, 2 hours, AC Characteristics: Alpha-beta alloy, good elevated temperature creep properties, good tensile properties, good stress rupture behavior, good thermal stability. Weldable, formable. Applications: Parts for gas-turbine engines |