Dutral® TER 4038 PL is an Ethylene - Propylene - Diene polymer produced by suspension polymerization using a Ziegler-Natta Catalyst. A non-staining antioxidant is added during the production process. Dutral® elastomers are characterized by excellent resistance to ageing and weathering, good resistance to both high an low temperatures, low permanent set values, good resistance to a large number of chemicals. Dutral® TER 4038 PL is a semi-crystalline terpolymer of medium-high molecular weight and medium diene content, supplied in pellet form. Thanks to this physical form, Dutral® TER 4038 PL can be advantageously used in polymer modification and in all the other applications in which continuous mixing is required. Main Applications: Automotive, cables, mechanical goods, buildings, appliances, polymer modification. Information provided by Polimeri Europa. Versalis is the Eni subsidiary containing the plastics and rubber businesses. |