Filler/Reinforcement: Glass Fiber, 15% Filler by Weight
Uses: Appliance Components; Automotive Applications; Automotive Interior Parts; Electrical/Electronic Applications
Agency Ratings: WRAS
RoSH Compliance: RoSH Compliant
Automotive Specifications: GM GMW3029P-PA6-GF15 Color 9697 Black; IMDS ID 3192311 Color: 9697 Black
Forms: Granules
Processing Method: Injection Molding
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlasticPA, Polyamide