Temper: As Sand Cast Casting Characteristics: High – Effect of Section Size; Medium – Fluidity, Casting Yield, Gassing; Low - Drossing, Shrinkage in Solidification Fabrication Properties: Excellent Suitability – Soldering; Good Suitability – Brazing Typical uses: Structural Castings; Nuts; Bearings; Bushings; Gears; High Pressure Hydraulic Equipment; Piston Rings; Pump Impellers; Pump Parts; Valve Bodies; High Pressure Steam Equipment Applicable Specifications: As Centrifugal Cast – Castings ASTM B271/B271M, Castings SAE J461, Castings SAE J462; As Continuous Cast – Castings SAE J462, Castings SAE J461, Castings ASTM B505/B505M; As Sand Cast – Castings SAE J461, Castings ASTM B584, Castings ASTM B763/B763M; Ingot - ASTM B30 |