MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Raschig Group PiMC 1949 Granite colors
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surface just prior to the molding of SMC/BMC. The PiMC 1949-series of granite colors were specially developed to give SMC/BMC parts the exclusive appearance of natural stone. Examples of (possible) applications are sanitary products and wall claddings.

Information provided by Raschig Group

Vendors:
Available Properties
  • Specific Gravity
  • Bulk Density
  • Particle Size, D 0.1, SATP-114, Malvern method
  • Particle Size, D 0.5, SATP-114, Malvern method
  • Particle Size, D 0.9, SATP-114, Malvern method
  • Storage Temperature
  • Elongation at Break, ASTM D790
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Abrasion, DIN 53799, [g] S42 paper, 500 turns
  • Gloss, 20°
  • Gloss, 60°
  • Gloss, 85°
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.