MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Mitsubishi Chemical Advanced Materials PE 500 HMW-PE Colors FG HMW-PE Colors FG High Molecular Weight Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: PE 500 HMW-PE Colors FG (Food Grade) is a versatile grade that offers a unique combination of stiffness, toughness, mechanical damping capabilities, great machinability, and moderate wear and abrasion resistance. In less demanding applications with respect to wear and impact resistance, PE 500 may present an economical alternative to standard UHMW grades. Due to these benefits and characteristics in combination with a EU 10/2011 and FDA 21 CFR § 177.1520 Food Contact compliancy, PE 500 HMW-PE FG components are primarily used in the meat and fish processing industry, but can also be found in a variety of mechanical, chemical, and electrical applications.

Vendors:
Available Properties
  • Density, ISO 1183-1
  • Water Absorption, ISO 62, Immersion
  • Water Absorption at Saturation
  • Hardness, Shore D, ISO 868
  • Tensile Strength, Ultimate, ISO 527-1/-2
  • Elongation at Break, ISO 527-1/-2
  • Elongation at Yield, ISO 527-1/-2
  • Modulus of Elasticity, ISO 527-1/-2
  • Flexural Strength, ISO 178
  • Compressive Yield Strength, ISO 604
  • Compressive Yield Strength, ISO 604
  • Compressive Yield Strength, ISO 604
  • K Factor (ISO), ISO 7148-2
  • Charpy Impact Unnotched, ISO 179-1/1eU
  • Charpy Impact, Notched, ISO 21304-2, double 14° notched
  • Charpy Impact, Notched, ISO 179-1/1eA, partial break
  • Coefficient of Friction, Dynamic, ISO 7148-2, Pin-on-disk vs. steel; 0.33 m/s
  • Sand Slurry, ISO 15527, based on TIVAR®1000 = 100
  • Limiting Pressure Velocity, 1 m/s; cylindrical sleeve bearings
  • Limiting Pressure Velocity, 0.1 m/s; cylindrical sleeve bearings
  • Electrical Resistivity, IEC 62631-3-1
  • Surface Resistivity per Square, ANSI/ESD STM 11.11
  • Dielectric Strength, IEC 60243-1
  • CTE, linear
  • Thermal Conductivity
  • Melting Point, ISO 11357-1/-3, DSC, 10°C / min
  • Maximum Service Temperature, Air, Continuous (20.000 hrs)
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2
  • Minimum Service Temperature, Air
  • Flammability, UL94
  • Oxygen Index, ISO 4589-1/-2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Mitsubishi Chemical Advanced Materials (former Quadrant Engineering Plastics Products)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.