MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.
Carlson C 200 Commercially Pure Nickel
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy; Pure Element

Material Notes: General Description

Carlson Alloy C 200 is commercially pure nickel, combining good mechanical properties with excellent resistance to many corrosive environments. This alloy retains its strength at high temperatures. It is tough and ductile at sub-zero temperatures.

C 200 is ferromagnetic and has one of the largest magnetostrictive effects of any commercial material. Its thermal and electrical conductivities are considerably higher than other stainless steels of nickel alloys.

Carlson C 201 is a restricted carbon (0.02% max.) version of C 200. It is preferred for exposure to temperatures above 600°F (315°C); and it is superior whenever creep strength is an important criterion.

Applications

C200 and C 201 provide excellent corrosion resistance to hot concentrated alkali (except ammonium hydroxide). These alloys exhibit good corrosion resistance to dry chlorine, fluorine, hydrogen chloride and hydrogen fluoride up to moderately elevated temperatures.

The corrosion resistance of both alloys make them particularly useful for maintaining product purity in food processing and in the production or processing of synthetic fibers, alkalis, fatty acids, soaps and detergents.

  • Chemical Processing – caustic processing and storage, chemical shipping containers, synthetic fiber productions, fluorine electrolysis.
  • Food Processing Equipment
  • Magnetostructive Devices
  • Aerospace and Missile components – rocket motor cases.

Information provided by Carlson

Key Words: UNS N02200
Vendors:
Available Properties
  • Density
  • Tensile Strength at Break
  • Tensile Strength, Yield
  • Elongation at Break
  • Tensile Modulus
  • Poissons Ratio
  • Shear Modulus
  • Electrical Resistivity
  • Curie Temperature
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Carbon, C
  • Copper, Cu
  • Iron, Fe
  • Manganese, Mn
  • Nickel, Ni
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.