MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
SABIC LNP™ STAT-LOY™ Compound D3000IEU6 Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP STAT-LOY D3000IEU6 Compound is a static dissipative Polycarbonate Copolymer based compound that has been designed towards ATEX compliant applications. The material has an optimized balance between surface resistivity and impact strength retention after hydro aging, and has excellent low temperature impact. The material is available in a wide range of dark and light colors, including UV stabilization.

Features: Electrostatic discharge (ESD),Hydrolytic Stability,Enhanced Low Temperature Impact,Enhanced Ductility,Easy Flow,Amorphous,General Purpose,Custom Color,Appearance & Durability,Dielectrics,Thin Wall,Colorable,Color Stability,Weatherable,UV Resistant,High Impact Resistance,High Flow,Heat Stabilized,Good Moldability,Good Mold Release,Ductile,Antistatic

Information provided by SABIC

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Density, ISO 1183
  • Water Absorption, ASTM D570
  • Water Absorption, ISO 62-1
  • Moisture Absorption, Injection Molding
  • Moisture Absorption, ISO 62-4, 23°C/50% RH/24 hrs
  • Moisture Absorption at Equilibrium, ISO 62-4, 23°C/50% RH
  • Water Absorption at Saturation, ASTM D570
  • Water Absorption at Saturation, ISO 62-1
  • Viscosity, ISO 1133, MVR cc/10 min
  • Viscosity, ISO 1133, MVR cc/10 min
  • Viscosity, ISO 1133, MVR cc/10 min
  • Linear Mold Shrinkage, Flow, SABIC method
  • Linear Mold Shrinkage, Transverse, SABIC method
  • Melt Flow, ASTM D1238
  • Ball Indentation Hardness, ISO 2039-1, H358/30
  • Tensile Strength, Yield, ASTM D638, 50 mm/min
  • Tensile Strength, Yield, ISO 527, 50 mm/min
  • Elongation at Break, ASTM D638, 50 mm/min
  • Elongation at Break, ASTM D638, 50 mm/min
  • Elongation at Break, ISO 527, 50 mm/min
  • Elongation at Break, ISO 527, 50 mm/min
  • Elongation at Yield, ASTM D638, 50 mm/min
  • Elongation at Yield, ISO 527, 50 mm/min
  • Tensile Modulus, ASTM D638, 50 mm/min
  • Tensile Modulus, ISO 527, 1 mm/min
  • Flexural Strength, ASTM D790, 1.3 mm/min, 50 mm span
  • Flexural Strength, ISO 178, 2 mm/min
  • Flexural Modulus, ISO 178, 2 mm/min
  • Flexural Modulus, ASTM D790, 1.3 mm/min, 50 mm span
  • Izod Impact Notched, ASTM D256
  • Izod Impact Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D4812
  • Izod Impact, Unnotched, ASTM D4812
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*3
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*3
  • Izod Impact, Unnotched (ISO), ISO 180/1U, 80*10*3
  • Izod Impact, Unnotched (ISO), ISO 180/1U, 80*10*4
  • Izod Impact, Unnotched (ISO), ISO 180/1U, 80*10*3
  • Izod Impact, Unnotched (ISO), ISO 180/1U, 80*10*4
  • Charpy Impact Unnotched, ISO 179/1eU, Edgew 80*10*4 sp=62mm
  • Charpy Impact Unnotched, ISO 179/1eU, Edgew 80*10*4 sp=62mm
  • Charpy Impact, Notched, ISO 179/1eA, Edgew 80*10*4 sp=62mm
  • Charpy Impact, Notched, ISO 179/1eA, Edgew 80*10*4 sp=62mm
  • Dart Drop, Total Energy, ASTM D3763, peak
  • Dart Drop, Total Energy, ASTM D3763
  • Dart Drop, Total Energy, ASTM D3763, peak
  • Dart Drop, Total Energy, ASTM D3763
  • Impact Test, ISO 6603-2, Multi-Axial Instrumented Impact Energy @ peak, 23°C
  • Impact Test, ISO 6603-2, Multi-Axial Instrumented Impact Energy @ peak, -30°C
  • Impact Test, ISO 6603-2, Multi-Axial Instrumented Impact Total Energy, 23°C
  • Impact Test, ISO 6603-2, Multi-Axial Instrumented Impact Total Energy, -30°C
  • Dart Drop Test, ASTM D3763
  • Dart Drop Test, ASTM D3763
  • Surface Resistance, ASTM D257
  • Surface Resistance, IEC 60093, ROA
  • Static Decay, FTMS101B, 5000V to <50V
  • Dielectric Constant
  • Dissipation Factor
  • Comparative Tracking Index, IEC 60112
  • CTE, linear, Parallel to Flow, ASTM E831
  • CTE, linear, Parallel to Flow, ISO 11359-2
  • CTE, linear, Transverse to Flow, ASTM E831
  • CTE, linear, Transverse to Flow, ISO 11359-2
  • Hot Ball Pressure Test, IEC 60695-10-2, PASS
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75/Bf, Flatw 80*10*4 sp=64mm
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75/Af, Flatw 80*10*4 sp=64mm
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, unannealed
  • Vicat Softening Point, ASTM D1525, Rate B/120
  • Vicat Softening Point, ASTM D1525, Rate B/50
  • Vicat Softening Point, ISO 306, Rate B/120
  • Vicat Softening Point, ISO 306, Rate B/50
  • Vicat Softening Point, ISO 306, Rate A/50
  • Vicat Softening Point, ISO 306, Rate A/120
  • Nozzle Temperature
  • Zone 2
  • Zone 3
  • Melt Temperature, Injection Molding
  • Mold Temperature
  • Drying Temperature, Injection Molding
  • Dry Time, Injection Molding
  • Dry Time, Cumulative; Injection Molding
  • Back Pressure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saudi Basic Industries Corporation; SABIC Innovative Plastics (GE Plastics)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.