MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Rogers Arlon CLTE-AT Commercial Ceramic PTFE
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.

CLTE-AT is a micro-dispersed ceramic PTFE composite utilizing a woven fiberglass reinforcement to provide the highest degree of stability, critical in multi-layer designs.

  • Ceramic/PTFE microwave composite
  • Mechanically more robust and more dimensionally stable than alternatives
  • High thermal conductivity
  • Lowest Insertion Loss in commercial class
  • Very low Loss Tangent (0.0013)
  • Tight Dielectric constant and Thickness tolerance
  • Electrical phase stability vs. temperature

Benefits:

  • Excellent thermal stability of Dk and Df
  • Phase stability across temperature
  • High degree of Dimensional stability required for complex, multi-layer boards
  • Excellent CTE in X, Y and Z

Typical Applications:

  • Automotive Radar & Adaptive Cruise Control Applications
  • Microwave/RF Applications
  • Phase/Temperature Sensitive Antennas
  • Phase Sensitive Electronic Applications
  • RF and Microwave Filters

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors:
Available Properties
  • Density, ASTM D792 Method A
  • Water Absorption, IPC TM-650 2.6.2.1
  • Outgassing - Total Mass Loss, NASA SP-R-0022A, Water Vapor Recovered
  • Outgassing - Total Mass Loss, NASA SP-R-0022A
  • Collected Volatile Condensable Material, NASA SP-R-0022A
  • Tensile Strength, IPC TM-650 2.4.18.3, Cross
  • Tensile Strength, IPC TM-650 2.4.18.3, Machine
  • Modulus of Elasticity, IPC TM-650 2.4.18.3
  • Flexural Strength, IPC TM-650 2.4.4, Cross
  • Flexural Strength, IPC TM-650 2.4.4, Machine
  • Compressive Modulus, ASTM D3410
  • Poissons Ratio, ASTM D3039
  • Shear Modulus, Calculated
  • Peel Strength, IPC TM-650 2.4.8, To Copper (1 oz./35 micron); After Process Solutions
  • Peel Strength, IPC TM-650 2.4.8, To Copper (1 oz./35 micron); After Thermal Stress
  • Peel Strength, IPC TM-650 2.4.8.2, To Copper (1 oz./35 micron); At Elevated Temperatures
  • Volume Resistivity, IPC TM-650 2.5.17.1, C96/35/90
  • Surface Resistance, IPC TM-650 2.5.17.1, C96/35/90
  • Dielectric Constant, IPC TM-650 2.5.5.3
  • Dielectric Breakdown, IPC TM-650 2.5.6
  • Dissipation Factor
  • Dissipation Factor
  • Dissipation Factor, IPC TM-650 2.5.5.3
  • Dissipation Factor, IPC TM-650 2.5.5.5
  • Arc Resistance, IPC TM-650 2.5.1
  • CTE, linear, IPC TM-650 2.4.41
  • CTE, linear, Transverse to Flow, IPC TM-650 2.4.24, z direction
  • Thermal Conductivity, ASTM E1461
  • Decomposition Temperature, IPC TM-650 2.4.24.6, Onset
  • Decomposition Temperature, IPC TM-650 2.4.24.6, 5 percent
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.