MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Zeus PI Glide™ High Lubricity Polyimide (PI) / PTFE Composite
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Unfilled

Material Notes: PI Glide™ PI / PTFE composite, is a high lubricity polyimide blend for applications that require lower surface friction yet do not require the performance of pure PTFE. PI Glide™ maintains broad chemical resistance and good dielectric properties in addition to its reduced coefficient of friction.

PI Glide™ is available in tubing and as a coating for over-the-wire (OTW, insulated wire) applications. For insulated wire, PI Glide™ provides a low-friction wire for easier deployment or insertion into tubing. With PI Glide™ tubing, inside diameters offer low resistance to inserted devices or tools (pushability) while the outside remains bondable without etching. PI Glide™ can also be produced in a layered composite construction with our conventional polyimide or with PI Glide™ alone. Composite layering polyimide and PI Glide™ allows users to further tailor polyimide tubing or coating properties.

Specific applications include catheters (vascular, structural heart, electrophysiology, urinary), lumen for guidewires, lead wire delivery devices, stone retrieval devices, and insulated wire.

Available in tubing, pull wires, low-friction lead (insulated) wire, and multi-layer construction.

Vendors:
Available Properties
  • Density, ASTM D792
  • Tensile Strength, Ultimate, ASTM D638
  • Elongation at Break, ASTM D638
  • Coefficient of Friction, ASTM D1894
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • Decomposition Temperature, in air
  • Flammability, UL94
  • USP Class VI
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.