MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
NRI Trident-Wrap®
Categories: Polymer

Material Notes: Trident-Wrap® Riser Reinforcement Kit repairs non-leaking natural gas risers exhibiting wall loss up to 80% @ <300 psi (20.7 bar) while eliminating atmospheric corrosion in accordance with DIMP. With 8 layers, this system enables one to repair corroded piping without shutdown or riser replacement. This operator qualified engineered system was designed to conform to and recognized by ASME PCC-2, ASME B31, ISO TS24817, DOT, API, and CSA Z662 standards for nonmetallic reinforcing solutions, thus ensuring product application integrity.

Typical Applications:

  • Corrosion repair on natural gas piping
  • Atmospheric corrosion
  • Riser reinforcement
  • New or old riser assemblies
  • Underground piping
  • Corrosion protection
  • Coating repair
  • Air to soil interface
Benefits:
  • No shutdown or relights
  • Simple application
  • No pipe replacement
  • Conforms to irregular shapes
  • No contractor required
  • Integrity management

Information provided by NRI® Innovative Composite Solutions

Vendors:
Available Properties
  • Tensile Strength, ASTM D3039, Axial
  • Tensile Strength, ASTM D3039, Hoop
  • Shear Strength, ASTM D5379, In-plane
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Processing Temperature, Application Range
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.