MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Parker Chomerics T-Wings Heat Spreaders
Categories: Other Engineering Material

Material Notes: Description: Chomerics’ family of thin heat spreaders provides a low-cost, effective means of cooling IC devices in restricted spaces where conventional heat sinks are inappropriate. T-Wing spreaders consist of 5oz. [0.007inch/0.18mm thick] flexible copper foil between electrically insulating films. High strength silicone PSA (pressure-sensitive adhesive) provides a strong bond to the component. The compliant nature of these “thermal wing” heat spreaders permits nearly 100% adhesive contact with non-flat package surfaces, optimizing thermal and mechanical performance.

Features/Benefits: Component junction temperature reduction of 10-20°C is common, Easily added to existing designs to lower component temperatures and improve reliability, Custom shapes available for complex designs, Low profile [0.33mm/0.013in] allows use in limited space environments, Easy peel and stick adhesion to all surfaces, including packages with residual silicone mold release, Offers low cost cooling for many package types, Low application force (<5psi/0.03MPa) minimizes risk of damage to component, Wide range of standard sizes, Pliable nature allows conformance to concave or otherwise non-flast surfaces for optimal thermal and mechanical performance, Light weight (0.039 oz/inch2), Standard parts are scored for easy forming and alignment, Easy removal for device replacement and Available die-cut on continuous rolls

Typical Applications: Microprocessors, Memory modules, Laptop PC’s and other high density, hand held portable electronics, and High speed disk drives.

RoHS compliant

Information provided by Chomerics

Vendors:
Available Properties
  • Thickness, Insulator Layer
  • Thickness, Visual, PSA Thickness
  • Thickness, Thermal Conductor
  • Thickness, ASTM D374, Total
  • Shear Strength, ASTM D1000, Lap
  • Shear Strength, ASTM D1000, Lap
  • Peel Strength, 60 min, 100°C, ASTM B571/D2861
  • Peel Strength, 1 min, 25°C, ASTM B571/D2861
  • Dielectric Strength, ASTM D149
  • Maximum Service Temperature, Air
  • Flammability, UL94
  • Shelf Life, Chomerics
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.