PELLETHANE® 2102-90AE elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with good damping capacity and good hydrolytic stability compared to other polyester based TPUs. Its typical applications seals, gaskets, belting, hose jacketing, tubing, animal ID tags and other fabricated products. Data provided by Dow Chemical. |