MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Vikas Ecotech CPE 135 A Chlorinated Polyethylene
Categories: Polymer; Thermoplastic; Vinyl (PVC); Chlorinated PVC (CPVC)

Material Notes: Chlorinated Polyethylene (CPE) is an elastomer, performs as an impact modifier for RPVC applications. It offers:
  • Excellent resistance to oil
  • Weathering properties
  • Resistance to aging
  • Good fire resistance properties
  • Excellent chemical resistance
  • Excellent compatibility with PVC & CPVC
  • Also an exceptional and economical impact modifier
Characteristics:
  • Fortune CPE is most suitable substitution of Acrylic impact modifiers without adjusting the processing parameter and formulations, resulting in an optimum performance: cost solutions
  • High surface gloss and smoothness
  • Good filler acceptance
Usages:
  • It can be used for producing PVC profiles
  • PVC pipes & fittings, cold curved pipe line
  • PVC sheets, PVC blowing boards
  • PVC extrusion boards
  • CPVC Pipes & fittings

Information provided by Vikas Ecotech LTD

Vendors:
Available Properties
  • Volatiles
  • Hardness, Shore A
  • Tensile Strength
  • Elongation at Break
  • Heat of Fusion
  • Chlorine, Cl
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.