MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
PoolKemie KEMIEPOX EL BLACK Casting epoxy resin
Categories: Polymer; Thermoset; Epoxy

Material Notes: Introduction: Two component room temperature vulcanizing compound based on suitable filled epoxy resins which cures with an appropriate hardener. KEMIEPOX EL Black is free from solvents and plastifiers, is very hard and has an excellent dimensional stability. In addition to this, it is characterized by a very good electric and mechanical resistance and chemical stability.

Application: KEMIEPOX EL BLACK is designed for manufacture of foundry models and moulds, insulation of electric circuits, creation of prototypes and insulation of acoustic equipments to avoid sound-waves scattering.

Information provided by Poolkemie

Vendors:
Available Properties
  • Specific Gravity, comp. B
  • Specific Gravity, A+B
  • Specific Gravity, comp. A
  • Viscosity, A+B
  • Storage Temperature
  • Hardness, Shore D
  • Tensile Strength, after post-curing
  • Elongation at Break, after post-curing
  • Flexural Strength, after post-curing
  • Compressive Strength, after post-curing
  • Volume Resistivity, after post-curing
  • Surface Resistance
  • Dielectric Constant
  • Maximum Service Temperature, Air
  • Glass Transition Temp, Tg, after post-curing
  • Cure Time, demoulding time (6mm. – 100 ml.)
  • Cure Time, complete curing
  • Pot Life, A+B, for 550 gr. mass
  • Gel Time, 6 mm, - 100ml
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.