MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Sandvik LDX 2101 Plate and sheet
Categories: Metal; Ferrous Metal; Austenitic

Material Notes: LDX 2101* is a duplex (austenitic ferritic) stainless steel with relatively low contents of alloying elements. The grade has high mechanical strength, similar to that of other duplex grades. Its good corrosion resistance is on par with that of most standard stainless steel grades. Combined, these properties can be utilized to optimize design with respect to strength, maintenance, durability and long term cost efficiency. LDX 2101 main characteristics:
  • High strength - approximately twice as high proof strength as austenitic stainless steels ASTM 304 and 316
  • Very good resistance to stress corrosion cracking
  • Good resistance to general corrosion and pitting
  • High energy absorption
  • Physical properties that offer design advantages
  • Ease of fabrication and good toughness
  • Very good weldability
Applications: General purpose applications and environments:
  • Building and construction
  • Storage tanks
  • Reinforcement bars
  • Water piping
Microstructure: The balanced chemical composition of LDX 2101 results in a microstructure containing approximately equal amounts of ferrite and austenite after annealing at a temperature of 1050°C (1920 F). Due to its relatively low alloying content, LDX 2101 is less prone to precipitaition of intermetallic phases than other duplex steels. The high nitrogen content results in rapid reformation of austenite in weld thermal cycles.

Information provided by Sandvik

Vendors:
Available Properties
  • Density
  • Hardness, Brinell, P
  • Hardness, Brinell, H
  • Hardness, Brinell, C
  • Tensile Strength, Ultimate, P
  • Tensile Strength, Ultimate, H
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate, C
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate, P
  • Tensile Strength, Ultimate, H
  • Tensile Strength, Ultimate, C
  • Tensile Strength, Yield, P
  • Tensile Strength, Yield
  • Tensile Strength, Yield, H
  • Tensile Strength, Yield, C
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield, P
  • Tensile Strength, Yield, H
  • Tensile Strength, Yield, C
  • Elongation at Break, P
  • Elongation at Break, H
  • Elongation at Break, P
  • Elongation at Break, H
  • Elongation at Break, C
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Poissons Ratio
  • Fatigue Strength
  • Toughness, P
  • Toughness, H
  • Toughness, P
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Carbon, C
  • Chromium, Cr
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Nitrogen, N
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.