Temper: Nominal Grain Size 0.050 mm Fabrication Properties: Excellent Suitability – Soldering; Good Suitability – Capacity for Being Cold Worked, Brazing; Fair Suitability – Butt Weld; Poor Suitability – Capacity for Being Hot Formed Common Fabrication Processes: Drilling; Knurling; Machining; Roll Threading Typical Uses: Hardware; Locknuts; Bushings; Caps; Couplings; Pipe Plugs; Regulators; Screw Machine Parts; Plumbers' Brass Goods; Plumbing Fittings Applicable Specifications: Bar – ASTM B140/B140M; Rod – ASTM B140/B140M; Shapes – ASTM B140/B140M |