MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Quaker Quintolubric® 855 Fire Resistant HFD-U Hydraulic Fluid
Categories: Fluid

Material Notes: Benefits:
  • Excellent lubrication properties
  • One viscosity grade works in systems designed for • ISO 46 or ISO 68 fluid
  • Non-toxic and non-irritating
  • Contains no hazardous ingredients
  • Product is readily biodegradable
Applications: QUINTOLUBRIC® 855 was designed to replace anti-wear, mineral oil-based hydraulic fluids as well as vegetable-based fluids and polyol esters. QUINTOLUBRIC® 855 can be used in or near fire hazards and in environmentally sensitive hydraulic applications without compromising the overall hydraulic system operation. QUINTOLUBRIC® 855 is based on high-quality, natural esters and carefully selected additives to achieve excellent hydraulic fluid performance. QUINTOLUBRIC® 855 does not contain water, mineral oil or phosphate ester. QUINTOLUBRIC® 855 is recommended for use in systems with a maximum operating temperature of 70°C (150ºF), in combination with partial refreshment by system leakage. QUINTOLUBRIC® 855 is used as received and pre-filtration is not necessary because the fluid is filtered during production. Its higher viscosity index compared with mineral oil makes it ideal for use at a wider temperature range. QUINTOLUBRIC® 855 also has good cold start-up properties and offers a higher viscosity at increased temperatures.

Information provided by Quaker

Vendors:
Available Properties
  • Density, ASTM D1298
  • Viscosity Measurement, ASTM D2270, Index
  • Kinematic Viscosity, ASTM D445
  • Kinematic Viscosity at 40°C (104°F), ASTM D445
  • Kinematic Viscosity at 100°C (212°F), ASTM D445
  • Vapor Pressure, 02551
  • Vapor Pressure, 02551
  • Total Acid Number, ASTM D974, [mg KOH/g}
  • Bulk Modulus
  • CTE, linear, ASTM D1903
  • Specific Heat Capacity, ASTM D2766
  • Thermal Conductivity, ASTM D2717
  • Pour Point, ASTM D97
  • Flash Point, ASTM D92
  • Ignition Temperature, DIN 51794, Autoignition
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.