MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Master Bond EP79FL Two Component Silver Nickel Conductive Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Very low volume resistivity
  • Outstanding flexibility
  • Cost effective
  • Silver coated nickel filled system
  • Withstands rigorous thermal cycling
  • Superior T-peel strength
Product Description: Master Bond EP79FL is a two component, electrically conductive epoxy for high performance bonding, coating and sealing. It utilizes silver coated nickel as the conductive filler and can be considered a cost effective alternative to more standard silver conductive epoxies. Most significantly, the epoxy is very flexible upon curing, which enables it to be used in applications involving rigorous thermal cycling and aggressive mechanical and thermal shocks. Additionally it has a high T-peel strength. EP79FL has a convenient one to one mix ratio by weight, and it cures readily at room temperature or more rapidly at higher temperatures. To optimize its properties, the recommended cure schedule is overnight at room temperature followed by a heat cure of 2-3 hours at 200°F. It is 100% reactive and does not contain any solvents or diluents, and has low shrinkage upon cure. Its electrical resistance is very low—less than 0.005 ohm-cm and its thermal conductivity is quite good. EP79FL can be applied readily with brush and has good flow properties. The system is conducive to thermal cycling over the exceptionally wide temperature range of 4K to +275°F, enabling it to be serviceable even in cryogenic applications. It has good chemical resistance to water, oils and fuels. Adhesion to metals, composites, glass, ceramics, vulcanized rubbers and many plastics is excellent. Parts A and B are both colored gray. Master Bond EP79FL adhesive is widely used in the electronic, aerospace, computer, semiconductor and electro-optic industries, among others.

Product Advantages:

  • Convenient mixing: one to one ratio by weight
  • Easy application: contact pressure only required for cure; adhesive spreads evenly and smoothly
  • Versatile cure schedules: ambient temperature cures or fast elevated temperature cures as required
  • Very low volume resistivity (<0.005 ohm-cm)
  • Cost effective alternative to silver filled epoxy

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Specific Gravity, Part B
  • Specific Gravity, Part A
  • Linear Mold Shrinkage
  • Tensile Strength
  • Elongation at Break
  • Tensile Modulus
  • Adhesive Bond Strength, Tensile lap, Aluminum to Aluminum
  • Peel Strength
  • Volume Resistivity
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg
  • Cure Time
  • Cure Time
  • Working Life, After mixing, 100 g batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.