MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Eastman Pamolyn™ 100 Oleic Acid
Categories: Fluid

Material Notes: Product Description: Pamolyn™ 100 Oleic Acid is an exceptionally high purity grade of oleic acid derived wholly from a tall oil fatty acid source. It is a low odor, essentially water white, low titer, oily liquid. Pamolyn™ 100 Oleic Acid is a unique commercial fatty acid in that it contains, typically, 90% oleic acid, all of which is in the naturally occurring cis-isomer form. Because Pamolyn™ 100 Oleic Acid contains only a low percentage of polyunsaturated acids, it has excellent oxidation resistance and color stability. Saturated fatty acids and unsaponifiables in Pamolyn™ 100 Oleic Acid are also outstandingly low. Pamolyn™ 100 is used in numerous cosmetic and personal care applications, functioning as an emulsifier or surfactant.

Application/Uses:

  • Building and Construction
  • Hot Melt Adhesives
  • Personal Care and Cosmetics
  • Solventborne Adhesives
Key Attributes:
  • Excellent color stability
  • Exceptionally high purity
  • Low odor level & uniform fatty acid composition
  • Low saturated acids and unsaponifiables content
  • Water-white initial color

Information provided by Eastman

Vendors:
Available Properties
  • Density
  • Total Acid Number
  • Gardner Color Number
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.