Product Description: PA 612, Heat Stabilized, Lubricated, Post Industrial Recycled Feedstock, Black Color Availability: North America Recycled Content: Yes Additive: Heat Stabilizer; Lubricant Features: Heat Stabilized; Lubricated RoSH Compliance: RoSH Compliant Appearance: Black Information provided by Ravago Manufacturing Americas |