MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Axiall HH-2000 Rigid PVC, Molding  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Georgia Gulf HH-2000 is a high heat/high flow injection molding grade PVC alloy with a price/performance niche between high flow vinyl and utility engineering thermoplastics. It combines excellent flow, toughness and heat deflection/sag characteristics that are a marked improvement over standard vinyl. In addition, HH-2000 has excellent heat and light stability, color hold and surface appearance, making it an ideal candidate for Class A appearance parts requiring good heat warpage resistance such as color computer monitor housings. Process Note: Drying of material for 24 hours at 140-160°F in a dehumidifying dryer is recommended to endure optimum processing characteristics.

Information provided by Georgia Gulf

Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued.

Vendors:
Available Properties
  • Specific Gravity, ASTM D-792
  • Linear Mold Shrinkage, ASTM D-955
  • Hardness, Rockwell R, ASTM D-785
  • Tensile Strength, Yield, ASTM D-638
  • Tensile Modulus, ASTM D-638
  • Flexural Strength, ASTM D-790
  • Flexural Modulus, ASTM D-790
  • Izod Impact, Notched, ASTM D-256
  • Izod Impact, Notched, ASTM D-256
  • Gardner Impact, per mil, 1/2" R Tup
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D-648
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D-648
  • Flammability, UL94
  • Oxygen Index, ASTM D-2863
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Axiall Corporation; formerly Georgia Gulf

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.