MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Celanese FORTRON 1140LC6 PPS, 40% Specialty
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

Material Notes: Fortron 1140LC6 is a 40% glass fiber reinforced material with a total chlorine content less than or equal to 900 ppm*. It offers excellent physical properties similar to those of the Fortron 1140L6 product.
FORTRON should in principle be predried. Because of the necessary low maximum residual moisture content the use of dry air dryers is recommended. The dew point should be =< - 30° C. The time between drying and processing should be as short as possible.
For subsequent storage the material should be stored dry in the dryer until processed (<= 60 h).

Information provided by Celanese Corporation.

Key Words: Low chlorine, 40% GF
Vendors:
Available Properties
  • Density, ISO 1183
  • Linear Mold Shrinkage, Flow, ISO 294-4
  • Linear Mold Shrinkage, Transverse, ISO 294-4
  • Tensile Strength at Break, ISO 527-2/1A, 5mm/min
  • Elongation at Break, ISO 527-2/1A, 5mm/min
  • Flexural Strength, ISO 178
  • Flexural Modulus, ISO 178
  • Izod Impact, Notched (ISO), ISO 180/1A
  • Izod Impact, Unnotched (ISO), ISO 180/1U
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact, Notched, ISO 179/1eA
  • Volume Resistivity, IEC 60093
  • Surface Resistance, IEC 60093
  • Dielectric Constant, IEC 60250
  • Dielectric Strength, IEC 60243-1
  • Dissipation Factor, IEC 60250
  • Comparative Tracking Index, IEC 60112
  • CTE, linear, Parallel to Flow, ISO 11359-2
  • CTE, linear, Transverse to Flow, ISO 11359-2
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1, -2
  • Deflection Temperature at 8.0 MPa, ISO 75-1, -2
  • Processing Temperature, hopper
  • Processing Temperature, cavity
  • Feed Temperature
  • Zone 1
  • Zone 2
  • Zone 3
  • Zone 4
  • Die Temperature
  • Melt Temperature
  • Drying Temperature
  • Dry Time
  • Moisture Content, Necessary low maximum
  • Injection Pressure
  • Hold Pressure
  • Back Pressure
  • Screw Speed
  • Screw Speed
  • Screw Speed
  • Hot-Working Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Ticona, Celanese Corporation

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.