MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Cabot ENERSILĀ® 2030 Silica Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Fumed silica additive for lead acid batteries
ENERSIL 2030 silica additive is suitable for use in hybrid Absorbent Glass Mat (AGM)-gel battery electrolytes. As an electrolyte additive, it can significantly reduce acid stratification, enable extended battery cycle life, improve cell-to-cell consistency and reduce battery pack maintenance. ENERSIL 2030 silica additive can also improve low temperature performance and cycle life in lead battery applications that require deep discharge. ENERSIL 2030 silica additive is designed specifically for use in lead battery applications. Each production lot is tested for dispersion stability characteristics to confirm quality consistency. ENERSIL 2030 silica additive maintains good dispersibility and stability in dispersions used in the production of hybrid AGM-gel batteries. ENERSIL 2030 silica additive is typically added to sulfuric acid electrolyte either by direct mixing or by preparing a 10 - 20 wt. % dispersion in water with or without dispersion stabilizers. Because of its unique morphology, ENERSIL 2030 silica additive is easier to disperse compared to other silica products and its dispersion viscosity remains stable during the battery filling process, providing uniformity of the gel distribution between the battery plates. ENERSIL 2030 silica additive is also suitable for use in gel lead batteries in various industrial and energy storage systems applications used in combination with solar and wind renewable energy sources. The key benefit of this product for these applications is its ability to provide excellent gel strength at lower silica loadings in the electrolyte versus other silica additives. Depending on the silica dispersion method and customer preference, ENERSIL 2030 silica additive can be provided either in fluffy or densed form.

Performance features:

  • Improves ease-of-processing and stability of water-based dispersions
  • Improves yield of high throughput electrolyte filling process
  • Improves battery cycle life in deep discharge applications
  • Helps maintain high discharge rates at low temperatures
Typical applications :
  • E-bikes
  • Lead battery powered electric vehicles
  • Energy storage systems (ESS)

Information provided by Cabot Corporation

Vendors:
Available Properties
  • Density, Tamped
  • Particle Mesh Size, ASTM D-1514, <0.02% residue
  • pH, ASTM E70-77
  • Specific Surface Area, ISO 9277, BET nitrogen
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.