MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
BYK Garamite® 1958 Rheological Additive for Coatings
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: General Description: GARAMITE™ 1958 is a unique rheological additive developed for a wide range of coatings systems. Compared to fumed silica and organoclays, GARAMITE™ 1958 provides improved sag (drainage) resistance, control of settling, metallic orientation, and stability. It is also more efficient and easier to handle in manufacturing (less dusty, higher bulk density and not sensitive to shear). Due to its patented mixed mineral thixotrope technology, GARAMITE™ 1958 provides these properties at lower viscosities than are seen with conventional thixotropes. Because the recovery properties obtained with GARAMITE™ 1958 are unique, it is recommended application properties such as sag resistance or spray trials be used instead of viscosity to evaluate the efficiency of GARAMITE™ 1958. GARAMITE™ 1958 use levels are system dependent. A loading ladder from equal loading to 20-40% less than your current thixotrope should be evaluated. Air release agents such as BYK®-A 555* and rheological enhancers such as BYK®-R 605* (typically added at 5-10% based on the weight of GARAMITE™ 1958), di-glycol amine, or water are beneficial in many systems and should be included in the overall optimization evaluation.

Benefits:

  • Dispersion Ease
  • Viscosity Stability
  • Shear Stable
  • Syneresis Prevention
  • Gel Time Stability
  • Settling Prevention
  • Drainage/Sag Prevention
  • Increased Efficiency

Information provided by Southern Clay Products

Vendors:
Available Properties
  • Bulk Density
  • Density
  • H2O, Water
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
former Southern Clay Products

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.