MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Aluminum 7055-T77511 Extrusions
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Material Notes: This alloy was specifically developed for use in compression-dominated structures and provides advantages over alloy 7150 in compressive and tensile strengths while maintaining other important properties such as fracture toughness and corrosion resistance.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Information provided by Alcoa and the reference(s).

Key Words: UNS A97055; Aluminium 7055-T7751; AA7055-T77511; Al7055-T77511
Vendors:
Available Properties
  • Density, AA; Typical
  • Density
  • Tensile Strength, Ultimate, LT Direction
  • Tensile Strength, Ultimate, Longitudinal Direction
  • Tensile Strength, Yield, LT Direction
  • Tensile Strength, Yield, Longitudinal Direction
  • Elongation at Break, LT Direction
  • Elongation at Break, Longitudinal Direction
  • Compressive Yield Strength, Longitudinal Direction
  • Fracture Toughness, KIC, T-L
  • Fracture Toughness, KIC, L-T
  • Aluminum, Al, As remainder
  • Chromium, Cr
  • Copper, Cu
  • Iron, Fe
  • Magnesium, Mg
  • Manganese, Mn
  • Other, each
  • Other, total
  • Silicon, Si
  • Titanium, Ti
  • Zinc, Zn
  • Zirconium, Zr
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.