MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Go Yen Chemical GOYENCHEM-920 Oil-Based Water Repellent Agent for Textile , Leather
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Intro: GO YEN CHEMICAL INDUSTRIAL CO., LTD. (GYC) Group always makes efforts to research and produce all types of water & oil repellent product. These high additional value series are already used to textile industries for many years. GOYENCHEM-920 belongs to solvent-based nano-fluorine structure. GOYENCHEM-920 do not use highly toxic solvent such as benzene, toluene or xylene for dilution. GOYENCHEM-920 can be widely used to various leather and textile materials processing. GOYENCHEM-920 provides good water & oil repellent? anti-stain and anti-dust performance, and still has good hand feeling?breathing ability and nature appearance after treated.

Advantages:

  • Provide good water & oil repellent performance for textile and leather
  • Provide anti-stain and anti-dust layer after treated
  • Suitable for use on various textile and fabric products
  • Can be used to several natural or synthetic leather
  • Good hand feeling
  • Excellent process stability
  • Good penetrability and wetting property
  • Excellent permeability
  • Do not affect material features after treated
Using Method
  • Suitable for various textile and leather processing
  • GOYENCHEM-920 can be sprayed and coated on leather and other surface
  • Diluted liquid can be used by aerosol can
  • Suggested dilution solvent : EAc?BAc?Hexane? Heptane?Butanone, the dilution can be adjusted 1 ~10 times by customer’s request.
  • Spray and coating back and forth twice and evenly.
  • Natural drying or heat drying (below 80?)

Information provided by Go Yen Chemical

Vendors:
Available Properties
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.